EVA 台湾台聚 UE629(华南仓提货)
冲击强度 | ASTM D-1709 | 430 | G/F50 | |
射出 | ASTM D-638/D-882 | 117 | kg/cm2 | |
VA含量 | ASTM USIFE | 18 | % | |
密度 / 比重 | ASTM D-1505 | 0.939 | g/cm³ | |
融化点 | ASTM D-2117 | 86 | °C | |
VICAT 软化点 | ASTM D-1525 | 64 | °C | |
熔融指数 | ASTM D-1238 | 2.5 | g/10min | |
低温易脆性 | ASTM D-746 | <-76 | ℃/F50 | |
硬度 | ASTM D-2240 | 31 | Shore D | |
铸膜成型 | ASTM D-638/D-882 | 180 | kg/cm2 | |
射出 | ASTM D-638/D-882 | 220 | % | |
铸膜成型 | ASTM D-638/D-882 | 750 | % | |
薄膜 | MD | ASTM D-638/D-882 | 250 | kg/cm2 |
TD | ASTM D-638/D-882 | 240 | kg/cm2 | |
MD | ASTM D-638/D-882 | 480 | % | |
TD | ASTM D-638/D-882 | 640 | % |
EVA/UE506/台湾台聚,VA含量6%,重要参数:熔体流动速率:8 g/10min密度:0.925 g/cm3硬度:43 维卡软化点:78 ℃脆化温度:-76 ℃。
EVA/UE510/台湾台聚,VA含量6%,重要参数:熔体流动速率:75 g/10min密度:0.926 g/cm3硬度:34 维卡软化点:68 ℃脆化温度:-76 ℃。
EVA/UE612-04/台湾台聚,VA含量19%,,重要参数:熔体流动速率:150 g/10min密度:0.94 g/cm3拉伸强度:5 MPa断裂伸长率:630 %硬度:34。
EVA/UE629/台湾台聚,VA含量18%,重要参数:熔体流动速率:2.5 g/10min密度:0.939 g/cm3缺口冲击强度:430 硬度:31 维卡软化点:64 ℃。
EVA/UE630/台湾台聚,VA含量16%,重要参数:熔体流动速率:1.5 g/10min密度:0.937 g/cm3缺口冲击强度:430 拉伸强度:16 MPa断裂伸长率:68 %。
EVA/UE631/台湾台聚,VA含量22%,重要参数:熔体流动速率:1.4 g/10min密度:0.942 g/cm3缺口冲击强度:374 硬度:36 维卡软化点:64 ℃。
EVA/UE659/台湾台聚,VA含量25%,重要参数:熔体流动速率:2 g/10min密度:0.947 g/cm3缺口冲击强度:444 拉伸强度:20 MPa断裂伸长率:87 %。